SP Cont. |
S ≥ |
FE ≥ |
SI ≤ |
AS ≤ |
CU ≤ |
ZN ≤ |
PB ≤ |
H2O ≤ |
SIZE ≥ |
|
S42 |
42% |
38% |
5.0% |
0.01% |
0.01% |
0.5% |
0.15% |
5.0% |
90% |
|
S38 |
38% |
34% |
8.0% |
0.01% |
0.01% |
0.5% |
0.15% |
5.0% |
90% |
|
S35 |
35% |
30% |
10.0% |
0.01% |
0.01% |
0.5% |
0.15% |
3.0% |
90% |
|
SIZE |
(0-5)mm/0-15mm/ or other size |
||||||||
|
PKG |
1000kg/bag or bulk |
||||||||
The core functions of Pyrite Ore for Smelting Additive Granules
In the roasting and recovery of non-ferrous metals are to provide a sulfur source, regulate the roasting atmosphere, supplement heat, and promote the conversion of metal oxides.
For oxide ores or metal oxides generated after roasting, pyrite decomposes at high roasting temperatures to produce various sulfur-containing substances. These sulfur-containing substances can undergo sulfidation reactions with metal oxides to form volatile or leachable metal sulfides, facilitating subsequent separation and recovery through distillation, flotation, or hydrometallurgical leaching.
The oxidative decomposition of pyrite consumes oxygen in the furnace, which can adjust the roasting atmosphere from a strongly oxidizing one to a weakly oxidizing or reducing one. Such an atmosphere is more conducive to the stable existence of non-ferrous metal sulfides.
For non-ferrous metal minerals with low calorific value, the addition of pyrite can ensure the continuous progress of the roasting process and maintain the reaction temperature stably within the range required by the process.